Material Notes:
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing expanded foams.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
Density 0.0300 g/cc
0.00108 lb/in³
Mechanical Properties Metric English Comments
Tensile Stress 0.125 MPa
18.1 psi
0.195 MPa
28.3 psi
0.250 MPa
36.3 psi
0.375 MPa
54.4 psi
0.700 MPa
102 psi
Flexural Strength 0.237 MPa
34.4 psi
0% E-por Content; DIN 53423
0.247 MPa
35.8 psi
60% E-por Content; DIN 53423
0.257 MPa
37.3 psi
100% E-por Content; DIN 53423
0.410 MPa
59.5 psi
DIN-EN 12089
Compressive Strength 0.140 MPa

@Strain 10.0 %
20.3 psi

@Strain 10.0 %
DIN-EN 826
0.175 MPa

@Strain 25.0 %
25.4 psi

@Strain 25.0 %
DIN-EN 826
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Commercial Status Europe
Cushioning 2.7
h/d=15; DIN 55471
Energy Absorption 16 J
Hysteresis at 70% compression, v=% mm/min; ISP 3386-1
Flexural Work to Break 0.227
0% E-por Content; DIN 53423
0.247
60% E-por Content; DIN 53423
0.25
100% E-por Content; DIN 53423
6.8 J
DIN-EN 12098