Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer BASF
Trade Name Elastollan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
ASTM D2240
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D412
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ASTM D-412
4.70 MPa

@Strain 300 %
682 psi

@Strain 300 %
ASTM D-412
Elongation at Break 870 %
870 %
ASTM D412
Tear Strength 51.0 kN/m
291 pli
ASTM D624
Tensile Set 75 %
75 %
at break; ASTM D-412