BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer BASF
Trade Name Elastollan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding applications. Cycle time improvements of up to 25% over standard polyester grade urethanes can be obtained with M-series grades. They exhibit excellent abrasion resistance, toughness, and resistance to fuels. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on molded plaques cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ASTM D2240
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM D412
Tensile Strength, Yield 8.50 MPa

@Strain 100 %
1230 psi

@Strain 100 %
ASTM D-412
19.7 MPa

@Strain 300 %
2860 psi

@Strain 300 %
ASTM D-412
Elongation at Break 590 %
590 %
ASTM D412
Tear Strength 135 kN/m
770 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 25
25
H-18 wheel; ASTM D-1044.
Processing Properties Metric English Comments
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Must be dried. Typical condition.
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.030 %
<= 0.030 %