BASF Lupranate® 5100 Isocyanate

Category Fluid
Manufacturer BASF
Trade Name Lupranate®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lupranate® 5100 Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lupranate® 5100 Isocyanate is an isocyanate blend of monomeric and polymeric MDI. Typical use is for flexible slab stock and molded Visco-Elastic memory foams.Information provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity 33 cP
33 cP
Vapor Pressure 1.33e-8 bar

@Temperature 25.0 °C
0.00000998 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 200 °C

@Pressure 0.000667 MPa
>= 392 °F

@Pressure 0.0967 psi
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
Color Amber
Composition Hydrolyzable Chlorine
<0.01%
NCO content
0.326