BASF Paliogen® Red Violet L 5100 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Paliogen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Paliogen® Red Violet L 5100 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Quinacridone pigment especially for bordeaux and maroon shade Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
Specific Surface Area 84 m²/g
84 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 5000 ohm-cm
>= 5000 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 5.0 - 8.0
5.0 - 8.0
Descriptive Properties Value Comments
Chemical Fastness (months) Butylacetate
4-5
Ethanol
3-4
HCL 2%
5
Methyl ethyl ketone
4
Mineral spirits
5
NaOH 2%
5
Solvenon™PM
3-4
Water
4-5
Xylene
4-5
Color Red Violet
Fastness to Overcoating 5