Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 5000 ohm-cm | <= 5000 ohm-cm | |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
Shakespeare Resistat® F9422 T040 Nylon 6 Monofilament Resistat F9422, MERGE T040 is composed of forty filaments of conductive nylon 6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface. .. |
|||
Electrical Resistivity | <= 5000 ohm-cm | <= 5000 ohm-cm | |
Shakespeare Sanstat® CN125 .89mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
Shakespeare Resistat® F9416 M040 Nylon 66 Monofilament Resistat F9416, MERGE M040 is composed of forty filaments of conductive nylon 6,6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Blue K 6911 D Color Additive Chemical Structure: Cu-phthalocyanine alpha stabApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applicat.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Blue K 7090 Color Additive Chemical Structure: Cu-phthalocyanine betaApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applications: .. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6920 Color Additive Chemical Structure: Cu-phthalocyanine, Alpha StablePhysical form: PowderApplication: Pigment for PaintsInformation provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6990 F Color Additive Description: Highly transparent Phthalocyanine blue pigment with neutral flopChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 7080 Color Additive Description: ß-phthalocyanine blue for economic formulationsChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate syste.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 9630 Color Additive Description: Transparent a-phthalocyanine blue –especially for effect shade Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 8690 Color Additive Description: Phthalocyanine green with excellent rheologyChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate sys.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 9361 Color Additive Description: Phthalocyanine green with extremely yellow and brilliant shadeChemical Structure: Cu Cu-phthalocyanine, brominatedPhysical form: PowderSuitable for: Baking systems, Waterborn systems, A.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliotan® Yellow L 1645 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systemsInformation provided by.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6700 F Color Additive Chemical Structure: Cu-phthalocyanine, Epsilon Application: Pigment for PaintsPhysical form: PowderInformation provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 8605 Color Additive Description: Bluish phthalocyanine greenChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 8731 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Blue L 6470 Color Additive Description: Transparent Indanthrone blue for effect and solid shades with high fastness propertiesPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, A.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Pink L 4790 Color Additive Description: Red pigment with very good weather fastnessSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red L 3880 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red L 3885 Color Additive Description: Transparent perylene red with a very clean shadSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Airdrying syste.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red Violet L 5100 Color Additive Description: Quinacridone pigment especially for bordeaux and maroon shade Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by .. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliotan® Yellow L 2045 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systems.Information provided b.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliotol™ Yellow L 0962 Color Additive Description: Opaque quinophthalone yellow with excellent rheologySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system and Airdrying systemsInformation prov.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding power Chemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Sicotan® Red L 2818 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Blue K 6902 Color Additive Chemical Structure: Cu-phthalocyanine alpha stab.Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applica.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6975 F Color Additive Description: Brilliant a-phthalocyanine blue with high color strength and excellent rheology in systems containing aromatic solventsChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: Po.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 7460 Color Additive Description: Metal free a-phthalocyanine blue especially for effect shadesChemical Structure: Cu-phthalocyanine, alpha-stab Physical form: PowderSuitable for: Baking systems, Waterborn systems, Acry.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Sico® Fast Red L 3855 Color Additive Description: Naphthol-AS-red pigment with good fastness properties in full shadeChemical Structure: Naphthol-AS-redSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Am.. |