BASF Pluracol® 1044 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 1044 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used in the preparation of polyurethane foams, adhesives, coatings, elastomers and sealants. Pluracol P410R and P710R are used in the preparation of one and two component polyurethane coatings, adhesives and elastomers.Information provided by BASF
Physical Properties Metric English Comments
Density 0.966 g/cc

@Temperature 60.0 °C
0.0349 lb/in³

@Temperature 140 °F
0.987 g/cc

@Temperature 37.8 °C
0.0357 lb/in³

@Temperature 100 °F
0.999 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
Viscosity 169 cP

@Temperature 60.0 °C
169 cP

@Temperature 140 °F
425 cP

@Temperature 37.8 °C
425 cP

@Temperature 100 °F
790 cP

@Temperature 25.0 °C
790 cP

@Temperature 77.0 °F
Molecular Weight 4000 g/mol
4000 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 27.5 - 30.5 mg KOH/g
STI 3007/3162
Unsaturation <0.1 meq/g
STI 3056