Physical Properties Metric English Comments
Viscosity 425 cP

@Temperature 37.8 °C
425 cP

@Temperature 100 °F
BASF Pluracol® 1044 Specialty Polyol
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used ..