Material Notes:
Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol 973, it gives good processability even in low-density, high water formulations which can meet automotive seating requirements. Pluracol 1421 is less reactive than Pluracol 945 and more reactive than Pluracol 538.Information provided by BASF
Physical Properties Metric English Comments
Density 0.992 g/cc

@Temperature 54.4 °C
0.0358 lb/in³

@Temperature 130 °F
1.00 g/cc

@Temperature 43.3 °C
0.0361 lb/in³

@Temperature 110 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 225 cP

@Temperature 54.4 °C
225 cP

@Temperature 130 °F
350 cP

@Temperature 43.3 °C
350 cP

@Temperature 110 °F
900 cP

@Temperature 25.0 °C
900 cP

@Temperature 77.0 °F
Molecular Weight 4800 g/mol
4800 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.030
<= 0.030
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 34 - 36 mg KOH/g
STI 3007/3162
Unsaturation <0.054 meq/g
STI 3056