Material Notes:
Description: Pluracol® 220 polyol is a high molecular weight, primary hydroxyl terminated polyol used in polyurethane elastomer and sealant formulations.Information provided by BASF
Physical Properties Metric English Comments
Density 0.980 g/cc

@Temperature 60.0 °C
0.0354 lb/in³

@Temperature 140 °F
0.985 g/cc

@Temperature 50.0 °C
0.0356 lb/in³

@Temperature 122 °F
1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
Viscosity 330 cP

@Temperature 60.0 °C
330 cP

@Temperature 140 °F
480 cP

@Temperature 50.0 °C
480 cP

@Temperature 122 °F
1300 cP

@Temperature 25.0 °C
1300 cP

@Temperature 77.0 °F
Molecular Weight 6000 g/mol
6000 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.060
<= 0.060
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
STI 3062
Descriptive Properties Value Comments
Color <40
APHA, STI 3057
Clear Liquid
Composition Na & K
<8 ppm, STI 3038
Hydroxyl Number 25.6 - 27.6 mg KOH/g
STI 3007/3162
Unsaturation <0.11 meq/g
STI 3056