Viscosity 1300 cP

@Temperature 32.2 °C
1300 cP

@Temperature 90.0 °F
BASF Pluracol® 1158 Specialty Polyol
Description: Pluracol® 1158 polyol is a polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. Wh..
Viscosity 1300 cP

@Temperature 25.0 °C
1300 cP

@Temperature 77.0 °F
BASF Pluracol® 220 Specialty Polyol
Description: Pluracol® 220 polyol is a high molecular weight, primary hydroxyl terminated polyol used in polyurethane elastomer and sealant formulations.Information provided by BASF
Viscosity 1300 cP

@Temperature 40.0 °C
1300 cP

@Temperature 104 °F
BASF Pluracol® SG-360 Rigid Polyol
Description: Pluracol® SG-360 polyol is a clear, light colored, low viscosity, sucrose/glycerine polyol. Pluracol SG-360 contains no nitrogen. The medium functionality polyol, when combined with su..