BASF Pluracol® 628 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 628 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used to manufacture a variety of sealants and elastomers.Information provided by BASF
Physical Properties Metric English Comments
Density 1.01 g/cc

@Temperature 54.4 °C
0.0365 lb/in³

@Temperature 130 °F
1.02 g/cc

@Temperature 37.8 °C
0.0368 lb/in³

@Temperature 100 °F
1.03 g/cc

@Temperature 25.0 °C
0.0372 lb/in³

@Temperature 77.0 °F
Viscosity 270 cP

@Temperature 54.5 °C
270 cP

@Temperature 130 °F
525 cP

@Temperature 37.8 °C
525 cP

@Temperature 100 °F
1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
Molecular Weight 4500 g/mol
4500 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 24.5 - 26.5 mg KOH/g
STI 3007/3162
Unsaturation <0.069 meq/g
STI 3056