Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 1.40 GPa
203 ksi
Charpy Impact Unnotched NB
NB
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
Vicat Softening Point 125 °C
257 °F