Physical Properties Metric English Comments
Density 0.998 g/cc
0.0361 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 8502 P BLK , 37.5% Filler Content
The following data represents the actual data obtained from Lot # 941101-5. The moisture content is 0.03%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Density 1.00 - 3.50 g/cc
0.0361 - 0.126 lb/in³
Average value: 1.08 g/cc Grade Count:174
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Density 1.00 - 1.04 g/cc
0.0361 - 0.0376 lb/in³
Average value: 1.02 g/cc Grade Count:26
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Density 1.00 g/cc
0.0361 lb/in³
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer
Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low..
Density 1.00 g/cc
0.0361 lb/in³
Momentive Performance Materials RTV12 Clear General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Density 1.00 g/cc
0.0361 lb/in³
LATI Latimass 75/4-04 D009 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne..
Density 0.998 g/cc
0.0361 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON MD000A PP
LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive.
Density 0.998 g/cc
0.0361 lb/in³
indicative
Solvay CATAFOR® F Surfactant
Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Soluble in water. Soluble in organic polar solvents.Solvent: Ethylene glycol 20%Available in: Asia Pacific, ..
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
Solvay GEROPON® TK 32 Surfactant
Description: GEROPON TK-32 is an effective dispersant in liquid formulationsChemical Name: SODIUM N-METHYL-N-TALL OIL TAURATECAS: 61791-41-1, 67-63-0Solubility in water: SolubleAvailable in: Asia Pa..
Density 1.00 - 1.15 g/cc
0.0361 - 0.0415 lb/in³
ASTM D792
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy
EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc.
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP
LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f..
Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Relative density
Suqian Unitechem Light Stabilizer 791
Chemical Name: Poly[[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidinyl)imino]-1,6-exanediyl[(2,2,6,6-tetramethyl-4-piperidinyl imino]])Characterization:..
Density 0.999 g/cc
0.0361 lb/in³
ISO 1183
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
Density 1.00 g/cc
0.0361 lb/in³
Dow Corning SYL-OFF® PMCPSL 9176 Anchorage Additive
Syl-Off® SL 9176 Anchorage Additive is one component of a multi-component silicone release system designing for coating on film substrates.Information provided by Dow Corning
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792, ISO 1183
DuPont™ Entira® AS500 Ionomer Resin
Entira™ AS MK400 is used to lower the static decay time and surface resistivity of polyolefins and other polymers. Entira™ AS MK400 can be precompounded or dry blended into polymers for extrusion,..
Density 1.00 g/cc
0.0361 lb/in³
Dow BETAMATE™ 73705 Polyurethane
BETAMATE™ 73705 is a one-part moisture curing polyurethane trim adhesive. It is formulated to provide adhesion to electro galvanized steel, phosphated steel, E-coated steel, and trim materials use..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Density 0.998 g/cc
0.0361 lb/in³
BASF D 2000 Polyetheramine
Formula: C5H9ClOCAS: 9046-10-0Description Polyetheramine D 2000 is a yellowish liquid, with an amine-like odor. It is partly miscible with water and other solvents. Synonyms: Polyetheramine D2000, ..
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® GL2100 ABS Good Flow Grade
Good flow, Easy processing, High glossInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.00 g/cc
0.0361 lb/in³
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee..
Density 1.00 - 2.20 g/cc
0.0361 - 0.0795 lb/in³
Average value: 1.76 g/cc Grade Count:71
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Density 1.00 g/cc
0.0361 lb/in³
Arkema Group Orgalloy® P 60AD Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.