BASF Ultramid® B3Z BK 30464 PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3Z BK 30464 PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid B3Z BK30464 is an impact-modified, pigmented black, unreinforced PA6 for injection molding.Applications: Impact-resistant articles, e.g. dowels.Information provided by BASF
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Yield 3.7 %
3.7 %
ISO 527
Flexural Modulus 1.75 GPa
254 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Processing Properties Metric English Comments
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Color BK 30464
Commercial Status North America