Material Notes:
Description: Ultramid® C40 L 01 is a lubricated copolyamide 6/66 grade of high viscosity for the production of monofilaments and blown film. Ultramid® C40 L 01 is well suited for the production of high transparency, nonsymmetric blown film with reduced curl. Its very low melting point compared to standard PA 6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. Product supplied in 2-2.5 mm cylindrical pellets.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Water Absorption 10.5 %
10.5 %
Saturation in water 23°C
Moisture Absorption at Equilibrium 3.2 %
3.2 %
23°C/50% RH
Viscosity Measurement 3.89 - 4.17
3.89 - 4.17
(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
240 - 260
240 - 260
(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
Thermal Properties Metric English Comments
Melting Point 192 - 194 °C
378 - 381 °F
ISO 3146
Decomposition Temperature >= 300 °C
>= 572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.080 %
<= 0.080 %
ISO 15512
Descriptive Properties Value Comments
Commercial Status Europe
Extractables <0.8 %
ISO 6427
Film Grade 1-3
BASF
Ignition Temperature >400°C
ASTM D1929
Lubricant 350 - 650 mg/kg
BASF