Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 100 Thick Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 100 Thick Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to fill voids and bonding areas. Bonds well to a variety of substrates and materials, formulated especially to plastics, metals and elastomers. Perfect for bonding rough and irregular surfaces and applications requiring up to 15 seconds of alignment and work time. BONDING SCHEDULES: Steel: 25-35 seconds, ABS: 10-30 seconds, Neoprene:
Physical Properties Metric English Comments
Brookfield Viscosity 1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
Brookfield LVF, Spindle 1-60 RPM
Mechanical Properties Metric English Comments
Shear Strength 5.00 - 10.0 MPa
725 - 1450 psi
polycarbonate; ASTM D1002/DIN 53283
6.00 - 9.03 MPa
870 - 1310 psi
PVC; ASTM D1002/DIN 53283
8.00 - 14.0 MPa
1160 - 2030 psi
ABS; ASTM D1002/DIN 53283
10.0 - 15.0 MPa
1450 - 2180 psi
neoprene rubber; ASTM D1002/DIN 53283
10.0 - 15.0 MPa
1450 - 2180 psi
acrylics; ASTM D1002/DIN 53283
15.0 - 22.0 MPa
2180 - 3190 psi
tensile; ASTM D1002/DIN 53283
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C
90.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 160 - 170 °C
320 - 338 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 51.7 °C
125 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.6 kV/mm
625 kV/in
Processing Properties Metric English Comments
Cure Time 0.083333 - 0.583333 min

@Temperature 24.0 °C
0.0013889 - 0.00972222 hour

@Temperature 75.2 °F
1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
full cure
Descriptive Properties Value Comments
Gap Filling 0.45mm
Copyright © lookpolymers.com All Rights Reserved