BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use above 150ºF a post-cure may be required. BC 5105 can afford consistent use to 300ºF if required. Does not contain VCHD or MDA. Uses: constructing vacuum form tools, injection and compression molds, RTM and RIM molds, and matched dies.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Brookfield Viscosity 2000 cP

@Temperature 23.9 °C
2000 cP

@Temperature 75.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 200 MPa
29000 psi
10 oz glass cloth laminate
Flexural Strength 234 MPa
34000 psi
10 oz glass cloth laminate
Compressive Strength 404 MPa
58600 psi
10 oz glass cloth laminate
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C
9.00 µin/in-°F
10 oz glass cloth laminate
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Pot Life 55 min

@Temperature 24.0 °C
55 min

@Temperature 75.2 °F
Descriptive Properties Value Comments
Mix Ratio 100:17 by weight, 100:20 by volume, resin/harder