Material Notes:
DP-11-83 is a low viscosity, quick setting, easy to use adhesive and/or casting material. This product was designed to bond together the MB1200 foam board to create desired dimensions in length, width and height. DP-11-83 has a working life of up to 13 minutes for casting applications. If used as an adhesive, it is workable for up to 16 minutes.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Brookfield Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.00050 cm/cm
0.00050 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 38 - 42
38 - 42
Tensile Strength, Ultimate 3.38 MPa
490 psi
Elongation at Break 800 %
800 %
Tear Strength 35.1 kN/m
200 pli
Processing Properties Metric English Comments
Cure Time 720 - 960 min

@Temperature 24.0 °C
12.0 - 16.0 hour

@Temperature 75.2 °F
demold time
1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
full cure
Pot Life 30 min

@Temperature 25.0 °C
30 min

@Temperature 77.0 °F
work life
45 min

@Temperature 25.0 °C
45 min

@Temperature 77.0 °F
gel time (180g)
Descriptive Properties Value Comments
Mix Ratio 100:90 by weight (resin/hardener)