Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BIW ASTM Class 2D1 Silicone Foam

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer BIW Silicone
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BIW ASTM Class 2D1 Silicone Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters.Information provided by BIW Isolierstoffe GmbH.
Physical Properties Metric English Comments
Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
DIN 53479 A
Mechanical Properties Metric English Comments
Hardness, Shore A 3 - 6
3 - 6
DIN 53505
Compressive Yield Strength 0.0150 - 0.0350 MPa
2.18 - 5.08 psi
25% Compression
Compression Set <= 80 %

@Temperature 100 °C,
Time 79200 sec
<= 80 %

@Temperature 212 °F,
Time 22.0 hour
50% Compression
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Standard Quality, All Colors
280 °C
536 °F
Highly Temperature Resistant Quality, Opaque, Grey, Blue
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Standard Quality, All Colors
Users viewing this material also viewed the following: