Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.250 g/cc | 0.00903 lb/in³ | True Density as as measured by gas displacement |
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | |
Pyrotek Pyrite Vacuum Formed Product Off White ColorApplicationsTap hole cones Riser sleeves Launder insulation Head boxes Ladle lining Pouring cups AdvantagesGood thermal shock resistance High strength/weight ratio Low thermal conduct.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | |
Pyrotek S-1100 Compressible Insulation Board The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insul.. |
|||
Density | 0.250 - 1.00 g/cc | 0.00903 - 0.0361 lb/in³ | available range |
MarkeTech Carbon Nanofoam Electrically conductive carbon nanofoams possess many of the properties of traditional aerogel material. These materials are available in the form of monoliths, granules, powders and papers. They ar.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | |
Sharadaa Ceramics Calcium Silicate Block Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | Foam |
Aptek DI-STRATE 95209 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Patch Radiators/SatelliteInformation provid.. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Density | 0.250 g/cc | 0.00903 lb/in³ | |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.250 - 0.300 g/cc | 0.00903 - 0.0108 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D1 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |