Material Notes:
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters.Information provided by BIW Isolierstoffe GmbH.
Physical Properties Metric English Comments
Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
DIN 53479 A
Mechanical Properties Metric English Comments
Hardness, Shore A 7.0 - 13
7.0 - 13
DIN 53505
Compressive Yield Strength 0.0350 - 0.0650 MPa
5.08 - 9.43 psi
25% Compression
Compression Set <= 60 %

@Temperature 100 °C,
Time 79200 sec
<= 60 %

@Temperature 212 °F,
Time 22.0 hour
50% Compression
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Standard Quality, All Colors
280 °C
536 °F
Highly Temperature Resistant Quality, Opaque, Grey, Blue
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Standard Quality, All Colors
Flammability, UL94 V-0
V-0
Self-Extinguishing Quality, Brown
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001 - 0.001 ohm-cm
0.0001 - 0.001 ohm-cm
Conductive Quality, Black