Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.300 g/cc | 0.0108 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo.. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials HFB Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials HG Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |
|||
Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Density | 0.300 g/cc | 0.0108 lb/in³ | |
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Density | 0.300 g/cc | 0.0108 lb/in³ | |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Density | 0.300 g/cc | 0.0108 lb/in³ | |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Density | 0.300 - 0.390 g/cc | 0.0108 - 0.0141 lb/in³ | Range |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D2 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Density | 0.300 - 0.340 g/cc | 0.0108 - 0.0123 lb/in³ | True, 3M QCM 14.24.6 |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials LG Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials PMF Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |