Material Notes:
Bapolan 6450 is a high impact polystyrene resin designed for injection molding applications requiring fast cycle times, superior impact and gloss. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose, housewares, and housings.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min
8.0 g/10 min
200'C/5,000g; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D-638
Elongation at Yield 43 %
43 %
ASTM D-638
Flexural Modulus, 1% Secant 2330 MPa
338000 psi
ASTM D-790A
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D-648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution