Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.1 MPa | 3500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPC-30T UV EXT 1148 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | TM R050-36 |
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with TP-95 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.1 - 40.7 MPa | 3500 - 5900 psi | Average value: 34.9 MPa Grade Count:78 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 24.1 - 34.5 MPa | 3500 - 5000 psi | ASTM D638 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Ineos 3950 Polypropylene Impact Copolymer Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2 in/min; ASTM D638 |
Ineos HP54-60 Flake Polyethylene Copolymer Flake This is a high density polyethylene copolymer flake which contains no additives and is not pelletized. It is designed for use in the plastic wood composite market.Information provided by Ineos Olef.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2 in/min; ASTM D638 |
Ineos TUB 121NTW HDPE TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi.. |
|||
Tensile Strength, Yield | 24.1 MPa @Temperature 23.0 °C |
3500 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos L12N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated impact copolymer polypropylene for injection molding and compounding applications. This material meets the requirements of the U.S. Food and Drug Administ.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Ineos L34N-00 Polypropylene Impact Copolymer Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Spartech PP5240 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Spartech Sound X Noise Abatement Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | >= 24.1 MPa | >= 3500 psi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.125" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D 638 |
Styrolution PS 6200/6201 HIPS Excellent toughnessDesigned for deep draw thermoformingUSP Class VI certifiedInformation provided by Styrolution |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Lubrizol Hipscon™ M-530 Static Control Polystyrene Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2"/min; ASTM D638 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2"/min; ASTM D638 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 6520A Injection Molding Polypropylene Impact CopolymerApplications: Closures, Housewares, Small Appliance ApplicationsFormolene 6520A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property b.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM-D638 |
CTC X-PRO CF 40 6002XT Polypropylene Copolymer, 40% Calcium Carbonate Filled X-PRO CF 40 6002 XT is a heat stabilized, 40% calcium carbonate filled polypropylene copolymer. It has an application in extrusion.Data provided by Composite Technologies (CTC). |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM Data |
Dow Prevail® 3150 ABS + Polyurethane PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
Aaron Industries AVPP C 200-4 Virgin Polypropylene, No Break A virgin copolymer polypropylene resin specifically designed for all high speed injection molding applications, featuring excellent toughness and strength. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | TM R050-36 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Tensile Strength, Yield | 24.1 MPa | 3500 psi | ASTM D638 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |
|||
Tensile Strength, Yield | 24.1 - 30.16 MPa | 3500 - 4375 psi | ASTM D-882 |
Saint-Gobain Norton® MFA Fluoropolymer Film Features/Benefits:Outstanding clarityPerformance from -254°C (-425°F) to 230°C (446°F)Outstanding flex life and stress-crack resistanceOutstanding anti-stick release propertiesExcellent electric.. |