Material Notes:
Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: Heavy duty industrial bags, industrial shrink film, construction and agriculture film.Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D-1505
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 24.1 MPa
3500 psi
10 in/min; ASTM D-882
Film Tensile Strength at Yield, TD 20.7 MPa
3000 psi
10 in/min; ASTM D-882
Film Elongation at Break, MD 350 %
350 %
10 in/min; ASTM D-882
Film Elongation at Break, TD 600 %
600 %
10 in/min; ASTM D-882
Secant Modulus, MD 0.159 GPa
23.1 ksi
0.1 mm/mm-min Initial Strain Rate; ASTM D-882
Secant Modulus, TD 0.179 GPa
26.0 ksi
0.1 mm/mm-min Initial Strain Rate; ASTM D-882
Dart Drop 8.46 g/micron
215 g/mil
ASTM D-1709; F<sub>50</sub>
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved