Bapolene® 122F Polyethylene, Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 122F Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. This product meets FDA standards for food contact applications.Applications: Industrial bags, shipping sacks, frozen food packaging, trash bags.Film properties below are based on a thickness of 37.5 µm and blow-up ratio of 2:1.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 37.6 microns
1.48 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 15.9 MPa
2310 psi
ASTM D882
Film Tensile Strength at Yield, TD 16.7 MPa
2420 psi
ASTM D882
Film Elongation at Break, MD 560 %
560 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Secant Modulus, MD 0.214 GPa
31.0 ksi
Value at 0.1 mm/mm-min Initial Strain Rate; ASTM D882
Secant Modulus, TD 0.248 GPa
36.0 ksi
Value at 0.1 mm/mm-min Initial Strain Rate; ASTM D882
Elmendorf Tear Strength, MD 6.70 g/micron
170 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 16.6 g/micron
422 g/mil
ASTM D1922
Film Tensile Strength at Break, MD 38.6 MPa
5600 psi
ASTM D882
Film Tensile Strength at Break, TD 29.6 MPa
4290 psi
ASTM D882
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003
Gloss 45 %
45 %
ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution