Bapolene® 222B Polyethylene Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 222B Polyethylene Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 222B is a butene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It complies with US FDA 21CFR177.1520.Applications: General packaging, garment bags, industrial packaging, and liners.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D-1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D-882
Film Elongation at Break, TD 700 %
700 %
ASTM D-882
Elmendorf Tear Strength MD 105 g
105 g
ASTM D-1922
Elmendorf Tear Strength TD 410 g
410 g
ASTM D-1922
Dart Drop Test 65.0 g
0.143 lb
ASTM D-1709
Film Tensile Strength at Break, MD 27.0 MPa
3920 psi
ASTM D-882
Film Tensile Strength at Break, TD 19.0 MPa
2760 psi
ASTM D-882
1% Secant Modulus, MD 172 MPa
25000 psi
ASTM D-882
1% Secant Modulus, TD 190 MPa
27500 psi
ASTM D-882
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved