Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBALLOY EP 23 ABS/PC, unreinforced, electro platable grade

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Barlog Plastics
Trade Name KEBALLOY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBALLOY EP 23 ABS/PC, unreinforced, electro platable grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ABS+PCInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
similar to ISO 62 test
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 240 °C
10 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1
Elongation at Break >= 25 %
>= 25 %
ISO 527-1
Elongation at Yield 3.5 %
3.5 %
ISO 527-1
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1
Charpy Impact Unnotched NB
NB
ISO 179-1eU
Charpy Impact, Notched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
Descriptive Properties Value Comments
Resin Type ABS+PC
Users viewing this material also viewed the following: