Material Notes:
BVC 1204-70 Clear has been designed as a general purpose extrusion compound for use in spiral hose, window profiles and applications where high gloss is required. This material offers excellent extrusion characteristics as well as adhesion to rigid properties. It also contains a UV stabilizer for light and heat stability.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 10.0 sec
70

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 13.7 MPa
1990 psi
ASTM D638
Elongation at Break 445 %
445 %
ASTM D638
100% Modulus 0.00469 GPa
0.680 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -42.5 °C
-44.5 °F
Impact Brittleness; ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified