Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bayshore Vinyl Compounds BVC 7200-75 Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Bayshore Vinyl Compounds
Trade Name BVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bayshore Vinyl Compounds BVC 7200-75 Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BVC 7200-75 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a smooth semi-gloss finish. Typical applications are wire coating, weather stripping, tubing, profiles and a variety of injection molded items.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78

@Time 10.0 sec
72 - 78

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 11.3 MPa
1640 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
100% Modulus 0.00527 GPa
0.765 ksi
ASTM D638
Tear Strength 40.8 kN/m
233 pli
ASTM D1004
Thermal Properties Metric English Comments
Brittleness Temperature -31.0 °C
-23.8 °F
Impact Brittleness; ASTM D746
Descriptive Properties Value Comments
Activated Carbon@90°C, % Wt Loss ASTM D1203
Weight Loss (%), ASTM D1239 0.7
Soapy H<sub>2</sub>O Extraction @ 50°C
14.9
Oil Extraction
28
Hexane Extraction
Users viewing this material also viewed the following: