Material Notes:
Information provided by Beijing Ranger Chemical Co.
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
Viscosity 8000 - 12000 cP
8000 - 12000 cP
Descriptive Properties Value Comments
Color APHA,= 50
Epoxy Equivalent g/eq 180-185
Inorganic Chlorine ppm, = 5
Saponifiable Chlorine ppm, = 100
Total Chlorine ppm, = 1700