Material Notes:
BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is a water dispersible acrylic enamel. HIGH PERFORMANCE ACRYLIC TOPCOAT is designed to be a low VOC and EPA compliant coating with excellent coverage and mar resistance. HIGH PERFORMANCE ACRYLIC is an ideal topcoat to replace solvent base acrylic enamel.Enviromental Advantages:BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics:Good exterior durabilityAvailable in satin to gloss finishGood hardness/impact resistanceWater is used for reductionExcellent performance on most plasticsWater is used for clean-upNon-HazardousAir dry or force curing preferredWide range of colorsCoating will not flash rust on bare metalShelf life of 1 year Unused paint can be returned to containerNon-Flammable UsesFiberglassSteelAluminum PlasticWoodPVCInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.04 g/cc
0.0377 lb/in³
Solids Content 39.2 %
39.2 %
by volume
43 %
43 %
by weight
Volatile Organic Compounds (VOC) Content 144 g/l
144 g/l
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Recoat, at 50% humidity
19.8 min

@Temperature 75.0 °C
0.330 hour

@Temperature 167 °F
Dust Free, at 50% humidity
45.0 min

@Temperature 75.0 °C
0.750 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Flexibility Good
Pencil Hardness HB
Salt Spray Good
Solvent Resistance Good; 20 double rubs
Theoretical Coverage 628 ft2 at 1 mil