Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Borealis
Trade Name Borclean™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antistatic additives or nucleating additives.Borclean HB311BF is especially suitable for biaxially oriented dielectrical film used in capacitors and manufactured for metallisable film.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
2.9 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
9.5 g/10 min

@Load 5.00 kg,
Temperature 230 °C
9.5 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Ash 0.0010 - 0.0020 %
0.0010 - 0.0020 %
ISO 3451-1
Thermal Properties Metric English Comments
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Electrical Properties Metric English Comments
Dielectric Constant 2.25
2.25
IEC 250
Descriptive Properties Value Comments
Calcium, ppm 5
from Anti-acid
Catalyst Residues, Aluminum ppm 2 to 4
Catalyst Residues, Chloride ppm 1 to 3
Catalyst Residues, Titanium ppm 1 to 3
Isotactic Index % 96
Borealis