BorsodChem ONGROCLEAN 10 anti-scaling agent

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer BorsodChem Rt.
Trade Name ONGROCLEAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BorsodChem ONGROCLEAN 10 anti-scaling agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ongroclean 10 is anti scaling agent for PVC polymerization. Composition of the material: Caustic solution of composite formed by bicycled phenols with formaldehyde. Low viscosity, odorless liquid.Field of application: Prevention of PVC scale formation on internal surface of reactors, condensers and pipes applied for suspension PVC production.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Solids Content 9.5 - 10.5 %
9.5 - 10.5 %
pH 12 - 13
12 - 13