Material Notes:
Description of product: Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable polyols it can be used as isocyanate component for producing rigid, semi-rigid insulating foams.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Viscosity 350 - 450 cP

@Temperature 25.0 °C
350 - 450 cP

@Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
wt %
Processing Properties Metric English Comments
Processing Temperature 20.0 - 25.0 °C
68.0 - 77.0 °F
Descriptive Properties Value Comments
Hydrolizable chlorine 0.3 max wt%
NCO Content, wt% 30 - 32