Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350 - 490 cP | 350 - 490 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1133 K (SBS) Linear Triblock Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | RPG30 |
Solvay ALKAMULS® EL 620 LI E Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€.. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | #3 SP @ 60 RPM; RP-0659 |
Solvay ALKAMULS® EL 620LI Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5A.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam STRUKSILON 8026 is used as a silicone stabilizer for the production of polyurethane shoe sole systems as well as other microcellular foams. It is especially recommended for shoe sole formulations ba.. |
|||
Viscosity | <= 350 cP @Temperature 25.0 °C |
<= 350 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E5 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | 350 - 550 cP @Temperature 125 °C |
350 - 550 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 350 cP | 350 cP | Mixed (SSA #15/7R, 100 rpm) |
Tra-Con Tra-Coat OPL6E Low Viscosity Adhesive Information provided by Tra-Con Inc. |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3660 Polyester, Pellet High elongation type UE3600 PaintUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Viscosity | 350 cP | 350 cP | dynamic |
Dow Corning ANTIFOAM B EMULSION Dow Corning® Antifoam B Emulsion is a water-dilutable, 10 percent-active silicone emulsion that is designed to control foam in aqueous systems.Information provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7600 Coating Syl-off® 7600 coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer.Information provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 200 Coating Low release at high speeds; high viscosityInformation provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 600 Coating Information provided by Dow Corning |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3 Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Viscosity | 350 - 650 cP @Temperature 23.0 °C |
350 - 650 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Viscosity | 350 - 550 cP @Temperature 23.0 °C |
350 - 550 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Viscosity | 350 - 550 cP @Temperature 23.0 °C |
350 - 550 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |
|||
Viscosity | 350 - 450 cP | 350 - 450 cP | |
Dow CYRACURE™ UVR-6110 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard base resin. It is useful in many applications in which low viscosity is not required: Metal decoration coatings Overprint varnishes Informa.. |
|||
Viscosity | 350 - 650 cP @Temperature 40.0 °C |
350 - 650 cP @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Viscosity | 350 - 500 cP @Temperature 35.0 °C |
350 - 500 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 90 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 350 cP | 350 cP | B Side |
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CR-30-40 MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable.. |
|||
Viscosity | 350 cP @Temperature 40.0 °C |
350 cP @Temperature 104 °F |
Solution, 25% in Dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | Part B |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |