Material Notes:
S-465 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It retains its excellent pourability even after compounding.Field of application: Ongrovil S-465 is suitable for both rigid and plasticized applications. It is recommended for the extrusion of rigid profiles and tubes, for injection molding of plasticized articles.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Apparent Bulk Density 0.510 - 0.570 g/cc
0.0184 - 0.0206 lb/in³
ISO 60:1977
Particle Size 63 µm
63 µm
10% below
250 µm
250 µm
1% above
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
ISO 1269:1980
Descriptive Properties Value Comments
# of Impurities max. 32 pcs/9dm2
K-Value 65±1
Pouring Time, sec (max) 23.5