Material Notes:
S-5258 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It retains its excellent pourability even after compounding. Field of application: Ongrovil S-5258 is primarily suitable for rigid applications. It is recommended for calendered or extruded films and sheets, injection molded or hollow articles such as fittings, opaque and transparent bottles.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Apparent Bulk Density 0.550 - 0.610 g/cc
0.0199 - 0.0220 lb/in³
ISO 60:1977
Particle Size 63 µm
63 µm
5% below
250 µm
250 µm
1% above
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
ISO 1269:1980
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
# of Impurities max. 20 pcs/9dm2
Fish-Eyes 10 pcs/dm2
K-Value 58±1
Pouring Time, sec (max) 22.5
Residual Vinyl-Chloride Content Max 1 mg/kg