Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Brandenburger
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Water Absorption >= 1.0 %
>= 1.0 %
24 hrs; DIN 53 495
Mechanical Properties Metric English Comments
Flexural Strength 100 MPa
14500 psi
EN 63
Compressive Strength 200 MPa
29000 psi
EN ISO 604
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
DIN 53 752
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52 612
Maximum Service Temperature, Air 230 °C
446 °F
Long Term
2500 - 3000 °C
4530 - 5430 °F
Short Term