Polymer Property : Density = 0.0578 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Celanese FORTRON ICE 506L PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron ICE 506L is a faster crystallizing version of Fortron 1140L6. It offers essentially the same characteristics of 1140L6 with improved crystallization efficiency for faster cycle times in comp..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron 1140L6 is an easier flow version of Fortron 1140L4. It offers essentially the same characteristics of 1140L4. Especially used for thin walled parts with long flow lengths. Applications made ..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D572
Haysite H254 Polyester Laminate
Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral
Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP 9X94104 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* 9X94104 is a compound based on Polyetherimide resin containing Glass Fiber.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Unitika UNILATE® 1 SC PET
Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Polyplastics Duranex® 750LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D 792
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled
PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l.
Density 1.60 g/cc
0.0578 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**)
25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
E-Polymers TEKAMID® TA250G60W , 62% Glass Fiber Reinforced PA66, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
Density 1.60 g/cc
0.0578 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ..
Density 1.60 - 1.75 g/cc
0.0578 - 0.0632 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
Density 1.60 g/cc
0.0578 lb/in³
cured; ASTM D794
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu..
Density 1.60 g/cc
0.0578 lb/in³
3M Scotchkote™ 162EP Epoxy Coating
3M Scotchkote Epoxy Coating 162EP has been specifically developed as 100% solids lining for the internals of tanks, vessels and other structures in contact with dirty water, sewage and oils.Informat..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® 551-GT30S PBT Resin
Glass fiber and mineral filled, flame retardant, low warpage, superior electrical performanceInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.60 g/cc

@Temperature 23.0 °C
0.0578 lb/in³

@Temperature 73.4 °F
ASTM D792
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Density 1.60 g/cc
0.0578 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 32960X078 0.078" (1.98 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flame Resistant Silicone PuttyAppearance: Gray colored, high viscosity gum on polymer ..
Density 1.60 g/cc
0.0578 lb/in³
Sat. Liquid
3M Novec™ 612 Magnesium Protection Fluid
Novec 612 fluid, dodecafluoro-2-methyl-3-pentanone or (CF3CF2C(O)CF(CF3)2, is a clear, colorless, and low odor fluid. Its properties, environmental profile, and margin of safety make it a sustainabl..
Density 1.60 g/cc

@Temperature 30.0 °C
0.0578 lb/in³

@Temperature 86.0 °F
3M Novec™ 7500 Engineered Fluid
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
DSM Arnite® TZ6 280 PBT-(GF+GB)40
20% Glass Reinforced, 20% Glass Beads Reinforced
Density 1.60 - 1.64 g/cc
0.0578 - 0.0592 lb/in³
ISO R 1184
Fainplast Compounds RE 140/1 Rigid PVC, Extrusion
Drain-pipes
Density 1.60 g/cc
0.0578 lb/in³
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East)
LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Guarniflon SC 1600 Polytetrafluoroethylene Seal
SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.