Braskem PH 3515 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PH 3515 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PH 3515 is a high melt flow rate homopolymer designed for injection molding. It is suitable for thin-walled injection molding parts. Its applications include: toys, caps and lids in general, household appliances, thin-walled parts, and easy mold filling.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 44 g/10 min

@Load 2.16 kg,
Temperature 230 °C
44 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM-D785
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM-D638
Elongation at Yield 8.0 %
8.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1700 MPa
247000 psi
ASTM-D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 119 °C
246 °F
ASTM-D648
Vicat Softening Point 152 °C

@Load 1.02 kg
306 °F

@Load 2.25 lb
ASTM-D1525