Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.290 - 7.47 J/cm | 0.543 - 14.0 ft-lb/in | Average value: 0.937 J/cm Grade Count:73 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plenco 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Izod Impact, Notched | 0.290 - 0.850 J/cm | 0.543 - 1.59 ft-lb/in | Average value: 0.647 J/cm Grade Count:3 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TF302 Wear Modified Acetal Resin PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TF304 Wear Modified Acetal Resin PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | |
Kuraray HYBRAR® A1 Thermoplastic Rubber-ABS Blend HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhi.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm @Thickness 3.17 mm |
0.543 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM-D256 |
Braskem PH 3515 HOMO Polypropylene Homopolymer PH 3515 is a high melt flow rate homopolymer designed for injection molding. It is suitable for thin-walled injection molding parts. Its applications include: toys, caps and lids in general, househ.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced A flame retardant PBT polyester with 45% glass reinforcement, mineral filled.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM-D256 |
Braskem H 203 HOMO Polypropylene Homopolymer H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
LNP ULTEM® JD7904 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |