Braskem RP 144 Coating Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem RP 144 Coating Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: RP 144 is a high melt flow rate random copolymer, designed for high speed coating equipments. This product features good processability, excellent gloss and weldability.Applications: Waterproofing of welded raffia bags.Information provided by Braskem
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792A
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 76
76
ASTM D785
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.800 GPa
116 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.350 J/cm

@Temperature 23.0 °C
0.656 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
10 N; ASTM D1525