Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.375 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **) PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -40.0 °C |
0.375 ft-lb/in @Temperature -40.0 °F |
ASTM-D256 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 23.0 °C |
0.375 ft-lb/in @Temperature 73.4 °F |
Practical Use; ASTM-D256 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1040 T8 V0 Flame Retardant Polypropylene Flame retardant class V0, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene PP homopolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 1040 TG Polypropylene, 20% Mineral Filled PP homopolymer 20% mineral fillerGood physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 1080 TG Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerExcellent stiffness, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 0.000 °C |
0.375 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -40.0 °C |
0.375 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem Prisma 2910 RACO Random Polypropylene Copolymer Prisma 2910 is a high melt flow rate random copolymer designed for injection molding applications. This product offers high impact strength at low temperatures and excellent processability. Its appl.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem RP 141 Injection Molding Polypropylene Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent .. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem RP 347 Injection Molding Polypropylene Description: RP 347 is a medium melt flow rate random copolymer designed for injection moulding. This product offers excellent transparency and gloss, very good stiffness/impact strength balance, ex.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem RP 144 Coating Polypropylene Description: RP 144 is a high melt flow rate random copolymer, designed for high speed coating equipments. This product features good processability, excellent gloss and weldability.Applications: Wa.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -20.0 °C |
0.375 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem Symbios 4102 Polypropylene Terpolymer Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) an.. |