Braskem TI2350C High Crystallinity Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI2350C High Crystallinity Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding.Process: CompoundingThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
2 in/min; ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256A