Material Notes:
Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive Interior Trim, Intricately Designed Parts, Thin-Walled Parts.Process: Compounding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength 31.0 MPa
4500 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2 in/min; ASTM D638
Flexural Modulus 1.41 GPa
205 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256A