Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TI4700P2 Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI4700P2 Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thinwalled parts, dairy containers, building and construction.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 26.9 MPa
3900 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2 in/min; ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256A