Mechanical Properties Metric English Comments
Tensile Strength 26.9 MPa
3900 psi
ASTM D638
Saint-Gobain Rulon® 1045 Bearing/Seal PTFE
Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy ..
Tensile Strength 26.9 MPa
3900 psi
2 in/min; ASTM D638
Braskem MV-501 Impact Copolymer Polypropylene
Description: Long term heat stability, nucleated, excellent processability.Applications: Suggested uses include compounding, thin-walled injection molding.Process: Injection Molding.This resin meets..
Tensile Strength 26.9 MPa
3900 psi
2 in/min; ASTM D638
Braskem TI4700P2 Impact Copolymer Polypropylene
Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thinwalled parts, dairy containers, building and const..
Tensile Strength 26.9 MPa
3900 psi
ASTM D638
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene
Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances..
Tensile Strength 26.9 MPa
3900 psi
ASTM D638
Americas Styrenics STYRON® 484 High Impact Polystyrene
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation pr..