Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TR3015WV2 High Crystallinity Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TR3015WV2 High Crystallinity Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding.Process: Compounding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDAInformation provided by Braskem
Physical Properties Metric English Comments
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 27.6 MPa
4000 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
2 in/min; ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256A